:ack:I had some faded purple plastic on my 97 sp and tried just about everything to bring it back to color, cleaners, polishes, plastic polishes, steel wool, etc, etc. Finally after rubbing super fast and hard with a rag and some metal polish, (extremely mad & frustrated) a small round piece of the plastic came back to color. trying to do it again, it seemed as though it was the heat from the friction that brought it back. So.... I pulled out my heat gun and SHAZAM!:hurray:
10 mins with a heat gun and my plastic looks VERY close to new. I found that the color gets a little modeled, but for the most part, it looks AWESOME! Try it for yourselves and let me know what you think!
10 mins with a heat gun and my plastic looks VERY close to new. I found that the color gets a little modeled, but for the most part, it looks AWESOME! Try it for yourselves and let me know what you think!